THERMOCOAT (SEC-L)/THERMOCOAT
Measurement for studs coating experiment - Page -3
Result page
1
2
3
4
Date-1/3/2006
28 Feb 2005 Pulling
Standards
KA
106.9
Anode Drop
521
STD DEV
1.16
VOLT
4.57
Cathode Drop
378
AVG
1.96
METAL
32
V(%)
59.10
BATH
18
Result: Decrease in Anode Drop
Rmarks: Std. No. 14,28,33,60 are still carring very less current along with these std. no. 34,37,66, also carry low current even after 10 days of pulling